SCANASYST-AIR-HPI
New ScanAsyst and PeakForce Tapping probes designed for applications in a high-volume environment on samples with high optical reflectivity that may cause laser interference and feedback into the AFM's optical position-sensitive detector. M
Tip Geometry: | Rotated |
Tip Height: | 3 - 8 |
Front Angle: | 15 |
Back Angle: | 1 - 24 |
Tip Radius (Nom): | 2 |
Tip Radius (Max): | 12 |
Tip Set Back (Nom): | 3 |
Tip Set Back( RNG): | 0-5 |
Cantilever Material: | Silicon Nitride |
Cantilever Thickness (Nom): | 0.58 |
Cantilever Thickness (RNG): | 0.53-0.63 |
Cantilever Geometry: | Special |
Cantilevers Number: | 1 |
Back Side Coating: | Reflective Al |